Defect: Flash residue | TPR injection toy
Cause: didn’t clean
Solution: check and clean inline, independent online inspector required during production.
Typical: * * * *
Rework difficulty: * *
Rework collateral risk: *
Defect: Flash residue | TPR injection toy
Cause: didn’t clean
Solution: check and clean inline, independent online inspector required during production.
Typical: * * * *
Rework difficulty: * *
Rework collateral risk: *