Product Inspection Service China


Expert Pre-shipment Inspection & Quality Control for Global Buyers

Bubbles on sealing surface | TPR squish ball


Defect: Bubbles on sealing surface | TPR squish ball
Cause: 1) High glue concentration causes the glue to dry too quickly, trapping air and forming bubbles; 2)redundant and uneven glue surrounding lid.
Solution: 1)Glue concentration must adjust with different seasons, higher in winter or low temperature, lower in summer; 2) glue on lid surrounded should be even when assemble to ball.
Typical: * * *
Rework difficulty: * * * * *
Rework collateral risk: * * * * *