Defect: Fake flow mark | TPR squish ball
Cause: Glitter powder can not melt completely into TPR material with grey color during injection
Solution: Currently has no good idea for grey color, and only found on grey color, so avoid grey color currently. Again, all bulk production must be proceed after production samples.