Defect: Missing paint | Electroplating glass plate
Cause: Electroplating before primer dry completely.
Solution: primer MUST be dry throughoutly, test with 3M tape before next step.
Typical: * * *
Rework difficulty: * * * *
Rework collateral risk: * * *